20061008

Curved mast -- tuning a mainsail

From: Philgeren@aol.com
Sender: Star45@yahoogroups.com
Date: Wed, 22 Nov 2006 06:58:53 EST
Subject: Re: [Star45] Curved mast -- advantage ??


Curving a mast so that it bends convex forward (concave aft) moves the luff edge of the sail forward and reduces the camber of the sail in the section where the mast is bent (if bent half way up the mast, the camber in the up/down center of the luff of the sail is reduced). In a blow, this reduces power, reduces leeway force, reduces weather helm, allows the boat to increase its speed.

Generally, the minimum position of mast bend is considered to be a curve equal to the luff curve designed into the luff edge of the mainsail. For very light air and for heavy air, maximum mast bend is used for maximum speed. For very light air, less camber makes it easier for air to stay attached to the leeward surface of the mainsail as the air passes aft. For medium air and for waves, where maximum power equates to maximum speed, minimum mast bend is used to get maximum designed camber.


By use of all the tuning controls on a mainsail, one can obtain a certain amount of control over the distribution of camber over the length of the mast, and there will be an optimum camber distribution for any particular sail and set of wind conditions. Pretty complicated to get it perfect, however outstanding sailors like Stuart Walker are on record as saying it is of paramount importance to use this against competitors who are using it. Otherwise, in a one-design competition they win.
My two cents.

Dave's musings about setting up and adjusting sails on R/C model Boat.

Dry sailing -set up.

Place the model in a stand. Head the model into them wind.

Things that can be moved, and adjusted: Mast step. Mast rake. Boom vangs. Shrouds. stays. Jumper stays. Head stay/jib stay. Sail shape - loose foot. out-hauls.

Attach the sails to the mast.

Set the sail winches in fully trimmed position while allowing sheets to be slack.

Stand the mast with standing rigging attached in the center step position.

Hook the jib swivel into the middle slot of the jib rack. {The jib boom needs to clear the mast.}

Connect the side stays to the chain plates and adjust so the mast is straight and vertical.

Connect the back stay to the back stay fitting.
The jib stay and back stay will need adjusting to set the mast in vertical position.

Move the out-haul of the sails along the boom to give the sails to have some "belly". Pulling the sails out along the boom flattens their shape. The belly (or shape) of the sails will be determined later and the sail shape will be determined by how windy it is.

Where you attach the sheets to the booms will take into account the type and adjustments available for the sail control. The booms should be full out (90 degrees to the center line of the hull) when the SCU is full out and then the booms should be just about over the center line when fully trimmed in. ( I see 10 degrees as suggested angle to center line). The length of jib sheet trimmed and the length of main sheet trimmed is a factor in setting up the sail control so the sails are coordinated properly when sailing. The SCU handles a much longer main sheet than the jib sheet. The use of jib traveler and mainsheet traveler can help position the sails when fully trimmed in. Unless two servos (SCU's) are used a single SCU has the task of coordinating the positioning of the jib and main.

Turn on the R/C and run the SCU.
Test out SCU setting with the sails full out and fully trimmed.

With the mast set up and sails adjusted roughly in position it time to launch and sail.
--
Setting Sail on the water.

Before launching TURN on the radio on the boat. I have seen many models set loose to sail with the on board receiver and sail controls not tuned on and very unhappy skippers watching as their model sails away towards the horizon.

The initial rigging and sail settings are based in getting the model to sail a strait line while close hauled (sails trimmed in) and sailing up-wind.

Properly trimmed the rig will allow the model to sail it self in a straight line with just a minor tendency to "round-up" (i.e. sail itself dead into the wind). If or example you find you are constantly pulling the tiller (i.e. rudder) hard over to pull the model back on course to keep from heading in to the wind your model has weather helm which means your mast and jib must be re-positioned. When tacking if your model stall's into the wind and won't tack? Try different rig setting.

--
Setting Sails
The art of tuning the rig on a sail boat is detailed in books written for racing yachts and boats.

"DINGHY SAILS"
by Jeremy. Howard-Williams

"The Best of Sail Trim:
A Selection of Articles from Sail Magazine"

"Sail Trim: Theory And Practice"
by Peter Hahne

My observations and commentary on tuning are from an amateur and are at best suggestions not professional advice.

Observation Number One!!
Model sails that are single panel loose footed sails rely on the shape of the sail established by the gap between the boom and the foot of the sail. Model sails with "shape" sewn into the sail fabric still are loose footed. Also the lift of the boom also factors in determining the shape and performance of the sails.

Hauling a sail into the center line and at the same time pulling down on the sail can flatten the fabric and kill the sail shape. I like to use travelers to position the sail to the desired point near the center line. Then you can set the point of maximum driving force and not wreck the sail shape.

On a big boat the skipper can changer the suit of sails to match the cut of the sail with the wind conditions. In the case of a model a skipper can change where the out-haul is along the boom, light air adding belly to increase the drive, heavy air pulling the sail out further changing the sail's airfoil.

The jib and mainsail work as a system. A skipper has all manner of combinations that may be set relating the two sails. If the models did not have jib clubs they could overlap the mainsail. So model sailors have to adjust the "slot" between the jib and the main to get the maximum driving combined air foil.

In heavy air you may want to close the slot and ease the main so that the jib slightly back-winds the main to help the model sail flatter (less heeling).

Don't forget on a model it is easy to rake the mast fore and aft to trim the sailing characteristics to match wind conditions.
--
A digital camera can be a terrific diagnostic tool for seeing what is happening on your model. You can look at pictures and spot misadjustments. Bends in mast, wrinkles in sails etc. Does you model's mast rake forward down wind? Is the back stay bending the top of the mast. How are the jumper/jenny stays adjusted do they balance the tensions between the jib and the back stay?
--
The late Manny Costa of RI always stressed, change one thing at a time to see what changes. He also stressed sailing a pair of models. One model being tuned and sailing against the second to see if the single adjustment improved performance.

Round-Robin racing in pairs is an excellent way to evaluate how your model performs.

Fiberglassing materials -- vacuum baging etc

Breather fabric is a lightweight, polyester blanket that provides excellent air passage within the vacuum envelope while it absorbs excess epoxy.
60" wide x 2.7 yd, 60" wide x 10 yd. 60" wide x 200 yd rolls:

Release Fabric is a tough, finely woven nylon fabric treated with a release agent. It is used to separate the absorber, breather and vacuum bag from the laminate in vacuum bagging operations. Excess epoxy bleeds through and is peeled from the cured laminate along with the release fabric. Peels easily and leaves a smooth textured surface, ready for bonding or finishing. 60" wide x 2 yd,. 60" wide x 10 yd rolls

Vacuum Bag Film is a Clear, heat-stabilized, modified nylon resin film, tough, stretchable film for high vacuum pressures. 60" wide x 2 yd, 60" wide x 10 yd,60" wide x 20 yd. 60" wide x 333 yd rolls:

Vacuum Bag Sealant; a mastic tape sealant for airtight seals between vacuum bags and molds. Easy to work with around difficult angles, patching small leaks in the system. 1/2" wide x 25' rolls:

Techniques Book on Vacuum Bagging, West System publishes this definitive guide to the principles and application of vacuum bagging techniques for laminating composite materials
with epoxy.

Fiberglass Mat is a Chopped Strand Fiberglass Mat, Offers great conformability with low cost.

Veil Mat 0.09 oz/sq ft

Fiberglass Mat, 3/4 oz/sq ft, 1.5 oz/sq ft, 2.0 oz/sq ft

Fiberglass Cloth 4-, 6- and 10-oz per square yard.

Dynel Fabric is a popular laminate fabric with great abrasion resistance used for museum-quality restoration work on wooden boats. It's strong and supple like a true woven fabric, with no fibers to irritate your skin.
Size Weight, 5 oz

Carbon Fiber lightweight, strong composite can strengthen any project while adding minimal weight.
Plain Weave 5.8 oz
Twill Weave 5.8 oz
Unidirectional 9 oz

Carbon Fiber Tape a unidirectional reinforcing tapes are used
to improve tensile strength and stiffness in one direction with minimal weight.

--

You can learn a lot about boat building by reading catalogs for example: www.jamestowndistributors.com/
Many of the same materials are also used in model boat building.

The Jamestown site has several links to model builders, AMYA and other organizations

Woode boat Construction -- glues and adhesives

John F. Howard (Star-45 discussion forum, July 31, 2006)

"Gorilla Glue does foam a bit, but nothing like foam-in-a-can and has minimum stink. Forget trying to smooth things out, the foam is very, very sticky and keeps growing until it sets up (about an hour) at which point it will still be a little soft (keep clamped for 3-4 hours). Any squeeze/foam out once hard, can be cut, chiseled or sanded smooth. Run a strip of tape along the edge of the glue line and most of the foam out will end up on the tape. The best joints are tight ones that use a minimum of glue. For narrow or thin pieces (planking), squeeze out a little puddle (just enough to use in 15-20 minutes) and use a Popsicle stick to spread along the edges. Wear gloves, the stuff stains and is sticky. GG is great for laminating larger areas (spread with an old credit card or playing card)."

"If you use epoxy resin such as West Systems (best, you can adjust the cure rate with the different hardeners) or one of the 30-minute or longer (5-15 minute never gets hard and remains rubbery) such as sold by Great Planes or Tower, stink will not be a problem. The polyester resin does STINK in a big way, it what you can smell in a new fiberglass hull.
CA glues are ok for "tacking" stuff in place until the epoxy sets up, but watch the fumes. CA will fail if used in a wet location for long and also cause a problem with the wood accepting stain. Work with plenty of ventilation and or respirator and wear gloves with any of the above glues and resins, staining of the skin and sensitivity, either skin and or breathing can occur."

"These are base on my experience with the glues mentioned (full size boats, cabinet work and models). Yellow glue such as Titebond or Elmers Carpenter Wood Glue (not waterproof) works fine when encapsulated with epoxy (cedar strip canoe builders use it all the time)."

{ http://groups.yahoo.com/group/Star45/ }

Phil Geren adds a warning note about Glue Fumes:
I have a serious allergic reaction to CA fumes - causes fluid to build up in the lungs, like pneumonia. I still use it, but with a fan blowing air between me and the work. Trying to avoid it.

Phil Geren on Gorilla Glue:2006 August 1
Is it rock hard or rubbery when dry?
I bought some, but have the same reservations as Dave M about foaming, trimming, and sanding. If it doesn't sand well, the finished product won't be as good as what I am aiming for.

Fiberglass Cloth, Matt -- polyester resins

This is a guide to assist the model builder in building model sailing boats from kits with fiberglass hulls and associated components.

"FIBERGLASS"

Fiberglass is the common name for glass reinforced plastics, GRP. The strands are produced in a non-woven cloth called matt and in a woven cloth called fiberglass cloth, boat cloth, tooling cloth and woven roving. After the cloth has been saturated with resin and the resin cured (hardened) we have fiberglass. Fiberglass matt and cloth are sold by the yard in small lots by retailers and by the pound by wholesale suppliers. Matt and cloth are designated in thickness by referring to their weights. Matt is weighed by the square foot with 3/4 to 3 oz. matt being most common. Cloth is also weighed but unlike matt it is weighed by the yard. Thus a 9 oz, cloth has the same glass content as 1 oz, matt. Matt and cloth have different handling characteristics and different conformability as well as different impact and strength factors. Working with matt using brush-on resin requires skill and experience to avoid developing one big mess of glass fibers and resin. You will find with a little practice that matt conforms well when worked with a resin-covered surface with a constantly wet brush. A matt called surfacing matt can be used to work the regular matt in place and squeeze out air bubbles and excess resin. This matt is hard to obtain other than from wholesalers. A layer of cloth works well for surfacing if you can stand the added weight. Fiberglass cloth put up in tape form is widely available. It is a convenient way of getting high quality cloth in small quantities. It is important for the glass resin combination to have as high a glass content as possible for strength. Fiberglass cloths used in boat building must have a special treatment called Chroming to make the glass compatible with the resin. Do not use industrial or auto grade fiberglass cloth unless it is treated.
Fiberglass (GRP) laminates will absorb water through the capillary action of the glass fibers. The problem of water absorption and surface abrasion is overcome in the molding stage by adding a specially formulated resin known as gelcoat. Although gel-coat is available clear, it is usually pigmented to give the surface resin a molded-in color. Polyesters and lay up resins can be pigmented giving the part a solid color throughout. This is an inexpensive way of molding color in but it presents two problems - hidden air bubbles within the laminate and exposing glass strands.

Working with Fiberglass "SAFETY" is Important !!

Always work in a well ventilated area. Resins, hardeners, and solvents are flammable and toxic. MEK60 is impact sensitive. Some people are ' especially sensitive to any and all components. Avoid excessive skin contact. Avoid inhaling concentrated fumes. Wash well and keep skin clean from these chemicals. chemicals follow manufacturers instructions. DO NOT SMOKE or have open flame around when working with fiberglass chemicals. Select an appropriate work area. Protect furniture, floors and other surfaces from spills and spatters {.o prevent permanent damage from these substances. Remember that the fibers of the fiberglass are irritants and commonly cause skin itching and irritation. When sanding, use a barrier cream or gloves, protective clothing and sanding mask and clothing and careful clean up methods as you work.

Fiberglass is just that, GLASS, and it will cut if you are not careful. When you sand, cut or trim anything made from fiberglass keep in mind that it can be as sharp as anything known to man.

Fiberglassing information and comments

Polyester resins are formulated in many make ups. To change the liquid resin to a solid you must add a hardener to catalyze the mixture. Whenever resin is referred to in this manual it is intended that it be properly catalyzed before use. The resin you choose for your model should be pre-accelerated. This resin will commonly have a purplish hue in the liquid stage and may change color to indicate states of cure. Resins should be at room temperature (60°-90°F. ) for curing. Among the polyester resins `available are the air, inhibited types. Lay up, spray, and gel-coat resins are formulated so their surfaces will not cure readily while exposed to air. This is advantageous if several layers of glass are to be laminated over a period of time. However, it may present a problem to the unsuspecting buildr who finds the surface of his resin "forever tacky". Sometimes, applying a layer of hard .bowling, alley wax will solve this problem. Gel- coat resins therefore, are' not used as a finish coating on completed boats because they are air-inhibited.

Finishing resin or hand-lay-up resin is commonly a waxed resin. When special waxes are formulated in the resin they will move to the surface as the resin cures. This is an advantage if this is the outer surface. If you want to bond to: this, surface you must first sand it thoroughly and then '" prepare, the surface with acetone or polyester solvent.

Polyester resins may be thinned with acetone and styrene. The common polyester hardener is methyl ethyl kettle peroxide (MEK60). -Resin and hardener 'must' be handled most carefully and in strict accordance with the manufacturers -instructions. The amount of hardener or activator in conjunction `with the room or ambient temperature determines the jel time and the cure' rate' of the resin. The jel time is the period that the resin remains liquid until it turns to a jelly just before curing hard. Resin has a "pot life" and is only workable for the time before it jels; this may vary from seconds to several minutes. CAUTION-DO NOT use too much hardener. Styrene will thin the resin' and become chemically part of the cured resin. Acetone will thin the resin but will evaporate during cure. Acetone will change the characteristics of the cured resin and may result in brittleness and other unwanted characteristics.

Polyesters may be filled with a 'number of components from sawdust to pecan shells. Most common fillers are Cabosil and micro-balloons and macro-balloons. This filling may make the resin thixotropic and filled resin may vary from a slurry to a heavy paste. Macro-balloons and micro-balloons are used to make a foam-like putty that will work as a flotation foam.

Polyester will bond nicely to polyester. We stress that surfaces must always. be cleaned and prepared for bonding. The bond between two fiberglass parts, such as keel and shell or hull and deck, will be enhanced if the interface between bonded surfaces is filled with a layer of saturated matt, cloth, or filled resin. Polyester resin is frequently used to bond to wood as a glue. However among wood glues, polyester rates poor. The initial bond to wood may look all right but it has a history of delaminating. We will not rule out its use for model building. However, there are better wood glues and the best of the waterproof glues are better, many epoxies.

Fiberglass is not at its best under tension. Spread or distribute any tension . load over a wide area. The same goes for compression loads that should be spread out also. This fiberglass found in models will tear if pulled on so always spread the load - more on this later.

You must remove all waxes in order to bond to fiberglass and you can reverse this and coat surfaces with hard floor waxes during building to protect surfaces from accidental spills. Also remember to use only resin-resistant tape such as Scotch brand Cellophane tape which is inert to resins; regular masking tape may be used if not in contact with resin or solvents.

Fiberglass has the outstanding feature that when molded in curves it has very high strength imparted to the part because of the curves. On smaller models the curves of the hull provide sufficient strength for the model. On larger models you will need stiffeners. These may be ribs or bulkheads which add support to the hull. These can be of the aircraft framework type. Another stiffening method is to make a sandwich. Here the strength of the GRP is achieved by laminating a light weight core between two layers of fiberglass.

From: "Mitch Martin" 2006 August 1

Working with WEST is similar to polyester resin, but it is stronger, doesn't smell bad, and hardeners can be selected for your application. For example if I was mixing the epoxy for glassing a hull that would eventially be painted I would select the extra-slow hardener 209 which has a pot life of 45 minutes. That's much longer than a polyester resin pot life. The down side is the cost, it's pretty pricy stuff. Another trick is to mix in the graphite powder and it gives the finish a carbon fiber look.

from John 2006 August 1

The pot life with the 105/209 is 40 min or so. I have used that
combination when doing vac bagging and it allowed plenty of time to wet
out the fabric on a 60" boat, then apply mastic, then the bagging
materials, then pull the air out. I have also done 72" long 10R's and had
no issues with the pot life. Now I am usually about 70 deg, so that slows
it down some too.

Now the 105/205 can be more in the 10 to 20 min range depending on temp.
Also how deep the container is that you mix the epoxy will influence the
cure time. Deeper is faster.

Billie Geisler's comments regarding Epoxy:

I use strips of cardboard scissored from breakfast ceral boxes for mixing and applying the epoxy. I use aluminum beer cans for containers. I cut the bottoms off about an inch up the can with a curved exacto knife. I find that I can get a pretty good mix of resin to hardener by cutting the mixer cardboard the same size, then use them to measure the epoxy and hardener.

I dip the cardboard mixer stick into the resin and scrape off all that will remain on the stick, after I wind up the strings, into the beercan. Then I use another fresh cardboard mixer stick, and dip it into the hardener to the same depth as I dipped the first stick into the resin. I let it drip once before I scrape it into the beer can. The difference in viscosity seems to get the ratio about right, even though it seems that no way is the little bit of hardener that stays on the dipper is going to be enough to work. The cardboard mixer sticks are inserted vertically into the resin and hardener, and scraped on the edge of the beer can.

You can pretty accurately go from a hot mix to a slow mix by simply varying the depth of the mixer stick in the hardener. It works on very small amounts, and about two dips from a half inch wide cardboard mixer stick will be enough for a plank on each side.

I use small jars to contain the epoxy components that I am working with, and label both the jar and the matching lid as resin or hardener. That way, if I happen to dip the used hardener dipper into the resin, or mix up the lids, I don't loose my whole supply. I like horshradish jars from Kraft.

Experiment with your epoxy before smearing it on your hull, as my epoxy is about 20 years old and the ratio of hardener to resin may work differently with yours. Just vary the depth of the hardener dip relative to the depth of the resin dip, until it works for you. It doesn't take long to learn to mix very small amounts with reliable cure results.

Billie Geisler's comments regarding Epoxy:

I use strips of cardboard scissored from breakfast ceral boxes for mixing and applying the epoxy. I use aluminum beer cans for containers. I cut the bottoms off about an inch up the can with a curved exacto knife. I find that I can get a pretty good mix of resin to hardener by cutting the mixer cardboard the same size, then use them to measure the epoxy and hardener.

I dip the cardboard mixer stick into the resin and scrape off all that will remain on the stick, after I wind up the strings, into the beercan. Then I use another fresh cardboard mixer stick, and dip it into the hardener to the same depth as I dipped the first stick into the resin. I let it drip once before I scrape it into the beer can. The difference in viscosity seems to get the ratio about right, even though it seems that no way is the little bit of hardener that stays on the dipper is going to be enough to work. The cardboard mixer sticks are inserted vertically into the resin and hardener, and scraped on the edge of the beer can.

You can pretty accurately go from a hot mix to a slow mix by simply varying the depth of the mixer stick in the hardener. It works on very small amounts, and about two dips from a half inch wide cardboard mixer stick will be enough for a plank on each side.

I use small jars to contain the epoxy components that I am working with, and label both the jar and the matching lid as resin or hardener. That way, if I happen to dip the used hardener dipper into the resin, or mix up the lids, I don't loose my whole supply. I like horshradish jars from Kraft.

Experiment with your epoxy before smearing it on your hull, as my epoxy is about 20 years old and the ratio of hardener to resin may work differently with yours. Just vary the depth of the hardener dip relative to the depth of the resin dip, until it works for you. It doesn't take long to learn to mix very small amounts with reliable cure results.

Star45 hull being fiberglassed


Covering Star45 model hull with fiberglass and epoxy resin

From: "John Fisher" racer577 at citystar.com
I have used the 3.2 oz satin weave on 7 boats now. The first was a single layer and now that hull is 4 or 5 years olds it is showing wear and tear. I went to using 2 layers to help with durability and to have more material for sanding. Another thing I like about the cloth is that is drapes very nicely and easily will cover the hull with one pc. On my 10R's I have used 2 yards folded in half to do the hull. On the star I was concerned that it would be too wide for a single yard. I ended up with more than enough material so I cut it on the diagonal.

The glassing starts by laying the glass over the hull. Then I smooth it out so there are no wrinkles. This may take a couple of min. Then I repeat with the next layer. Once the glass is smooth, time for epoxy. I used the 209/105 west systems combination. I used about 10 pumps of material.

I start applying resin to the middle of the bottom with a cheap paint brush. Then I work my way out to the edges of the bottom. Next I do the sides. You need to use lots of resin and dont pull too much or you will pucker the cloth. Once everything is wetted out I go back with a squigee and remove the excess resin. Dont get to carried away or the cloth will go dry again. If in doubt of how this should look practice on a spare block of wood first to get a feel for how the cloth looks as you take out resin.

I did the glassing at about 8 pm and with the 105/209 the resin is still green at 7 am the next morning. When green the glass can be trimmed with a #11 blade in a hobby knife. Then wait another day or two until sanding for full cure. I dont like to do much sanding, instead I try and do most of my fairing by using a thick primer and sanding most of it off between coats. For a clear boat I use polyurethane for a top coat.

Stand for tuning finished model

John Fisher sent these in. It might spark some thought for other people as well. He does not claim to have come up with this design, You can use any materials that you have handy, He has a mill and a welder, so his ended up in aluminum. these stands have been built from PVC and Copper pipe as well.

The stand has a vertical tube that is the pivot for direction. This way the boat can feather into the wind. If the ground is soft enough where you sail it can be pushed into the ground. Works fine in so-cal but not very well in colorado. Next there is a H shaped part that holds the boat. His are machined and welded aluminum, but he has seen this part done with copper water pipe or PVC pipe. He added the foam for insulating water pipes to prevent the boat from being scratched. The H should be able to rotate. This allows the boat to heel in the stand when force is applied to the sails. Connect the two and you have your stand. On his stand the connector is a pcs of 1/2" diameter SS tubing bent 90 deg. It provides both motions needed.

tunstand051sml

The boat shown is a hard chine 10R Class called the Diamond.

tunestand71sml.jpg
John Fisher has cutting files available for hard chine model 10R Class as well.
They go fast :-). John's 10R Class carries 1500 sq in of sail, is 65"
long and only 9" wide.

Star 45 Setting Sail -- on-line "How To Sail" resources

From: "Don Keeney" <1keyknee@281.com>
Date: Sun, 19 Nov 2006 15:39:26 -0600
Subject: [Star45] Sail Trim

A great place to learn about sail trim and sailing in general.
http://www.sailingusa.info/sail_trim.htm

Don Keeney
Star 45 Class Secretary
--
Outstanding recommendation. Wonderful site. full of photographs and all sorts of instructional materials. Pictures of tells and how to read them:)

Another must place to visit (you can try out your sailing skills):
National Geographics Interactive Sailing:

Master rudder and sail to get your boat going as fast as possible no matter what direction you're sailing in-or which way the wind's blowing.

Controls available:

Sail Adjuster: Use the left sliding controller to rotate the sail in relation to shifting wind (shown as arrows). When you cross the path of the wind, your sail will swing to the opposite side.

Rudder Adjuster: Using the right sliding controller, steer to port (left) or starboard (right).


Uncle Dave

modern sail materials, North Cloth - Industrial Fibers

by Peter Mahr and Brian Doyle
http://na.northsails.com/North_Cloth/industrial_fibers.html

Almost every piece of modern sailcloth begins life as an industrial fiber. While the brand names of many of these fibers are well known to sailors, their basic properties are less well understood. The characteristics of these fibers are an important factor to consider when choosing sails for your boat. Over the past few years there have been some significant developments in high performance fibers that have applications in sailcloth. The result is a greater variety of options for performance sailcloth makers and their customers, allowing them to select the blend of performance, durability and cost that best suits their needs.

Polyester
Polyester is today's "classic" sailcloth fiber. It is often called by the Dupont trade name DACRON® although there are other suppliers of polyester yarn used in sailcloth. Polyester is widely used for its combination of reasonably low stretch, good strength, low cost and durability. Because it can be heated and shrunk during weaving to form a tight, stable woven cloth, polyester woven sailcloth remains a good choice for cruising sails and certain racing sails. Polyester is available in many types. Dupont’s Type 52 is a "high-tenacity" premium fiber offering a balance of higher strength, lower stretch and maximum shrinkage. Other premium polyesters, with comparably excellent properties at more attractive prices, are now available from Asian and European suppliers. Their use in sailcloth has increased over the last few years at the expense of Dacron.

Nylon
Nylon is used for most downwind sails because it is strong and light. Nylon is relatively stretchy, allowing it to absorb shock loads and making it easier to fly and more stable in wavy seas than a polyester material would be. Dying this fiber is easier than any other and it is often available in a variety of colors.

Aramids
A popular class of high performance fiber in laminated sailcloth is the Aramids. The most well known aramids are Kevlar™ (a Dupont trademark) and Twaron™ (made by Teijin/Twaron of Japan). Sails made with aramid fiber are lighter than woven Dacron or Polyester laminates, and have greater effective wind ranges. The tradeoff is higher cost and shorter sail life. The stiffer Aramid fiber is more susceptible to sunlight (UV) damage and breakdown due to folding and flogging.

Aramids are produced in a number of different styles, with different balances of stretch, flex strength, weight and cost. High modulus (low stretch) types such as Kevlar 49 and Twaron 2200 are the most appropriate choice for racing sails. A variation of Kevlar called “Edge” was promoted a couple of years ago because it had slightly higher initial modulus. North’s testing revealed that this effect disappeared almost immediately with use. This type has since been discontinued.

Another aramid fiber is Technora, which is similar to medium modulus Kevlar in chemistry and performance. Initially it has a bit higher strength but loses strength more rapidly in UV making it similar in durability in most applications. It is commonly seen with a black coating, which is intended to provide some UV screening.

Vectran
Vectran is a LCP (liquid crystal polymer) fiber sold by Hoechst. Vectran’s stretch resistance is nearly as high as a standard modulus aramid, and it is somewhat stronger when new. It differs from aramids in its chemistry and has somewhat better flex resistance as long as it is shielded well from UV. Under UV exposure, it degrades more rapidly than aramids and far faster than Spectra/Dyneema.

Carbon Fiber
First used successfully in the 1992 America's Cup, carbon fiber laminates provide exceptionally low stretch and light weight at the expense of higher cost and somewhat shorter life span compared to an aramid sail. Careful R+D and on the water testing is critical with this fiber. Carbon is available in a wide variety of types, only a few of which can tolerate the flexing seen in normal sail use. Laminating techniques are also very critical to get the available high performance as well as to achieve the best possible durability. Experience over that last few years on top boats with 3DL carbon and carbon/aramid sails has been very positive and the fiber is seeing increasing use by more types of boats.

Spectra/Dyneema*
Spectra, and its European counterpart Dyneema, offer even lower stretch, higher strength, better UV resistance and much less strength loss in flex than Kevlar. However, Spectra/Dyneema sails stretch (creep) under long-term load, which makes them unacceptable for racing sails. After considerable development, this fiber is now used with excellent results in sails for large performance cruising boats.

* Note: We use the somewhat awkward ‘Spectra/Dyneema’ reference since we employ the two fibers almost interchangeably and sometimes in the same piece of cloth

PBO
At the top of the theoretical performance list is PBO, a fiber made by Japanese company Toyobo. This fiber has been used for a number of years in both 3DL and paneled sails. It has proven to be somewhat better than an aramid sail in performance when new but degrades rapidly under the combination of UV and flex. Because it is a very expensive fiber, its use in sails has all but disappeared in favor of the even higher performance and more durable carbon option.

PEN
PEN is a fiber with stretch between polyester and aramid and with slightly higher strength than polyester but far less than aramid. That combination and a cost approaching aramid have meant that this fiber has limited application in sails. It has been ruled to be polyester and as such can be used in one-design classes that limit their sails to polyester.

Summary
New fibers continue to come out of the labs. Some will become standards while others will disappear. Despite the promise of these exciting new fibers, design still plays a vital part in their successful application in your sails. Simply inserting a spicy new fiber in a poorly engineered fabric or sail design is a formula for failure. Similarly, enough of the fiber must be used to handle the sailing loads and the abuse it will take in tacking, flogging and handling. Low stretch has always been desirable in selecting fibers for sailcloth but this is only one element in a sail's performance. It is ultimately the combination of fiber, fabric and sail design that makes for a winning sail.

Fortunately for North our 3DL molded sailmaking process allows us to produce a test sail from a new fiber within a few days of its arrival at our factory in Nevada. This has allowed us to quickly evaluate new offerings and to remain the industry’s technological leader.

Pictures of International Star Class Yachts under sail








Photographs by Fried Elliott
PO Box 940010
Plano, TX 75094

email: fried @ friedbits.com